In short: Design printed ceramic parts with even, moderate wall thickness, generous radii and no sharp internal corners. Give hollow parts drain holes for uncured slurry, allow for sintering shrinkage and put critical tolerances and datums on the drawing so finishing and measurement can be planned.
Design rules at a glance
| Feature | Starting value | Notes |
|---|---|---|
| Minimum wall thickness | mm | Thinner is possible for small, unloaded features |
| Thickest solid section | Keep as thin as the function allows | Sections beyond about 15 to 20 mm are difficult to debind |
| Minimum hole diameter | mm | Smaller holes are possible as through holes |
| Minimum channel diameter | mm | Channels must allow slurry to drain |
| Internal radius | mm or larger | Sharp internal corners concentrate stress |
| Drain holes in hollow parts | mm, at least two | Placed at the lowest points in print orientation |
| Tolerance as sintered | ± value or percentage | Tighter tolerances by finishing |
| Tolerance after finishing | ± µm | Depends on feature and material |
These are starting points. Your engineer confirms the values for your material and geometry during the design review.
1. Keep walls even
Large jumps in wall thickness heat and cool at different rates during debinding and sintering. That creates stress and can crack the part. Core out thick sections or replace them with a lattice.
2. Round every internal corner
Ceramics do not yield, so a sharp internal corner concentrates stress until the part breaks there. Add radii to internal corners and fillets where walls meet.
3. Plan for shrinkage
The part shrinks during sintering. We scale the print file to compensate, but features with very different sizes can shrink slightly differently. Mark critical dimensions so we can measure them and finish them if needed.
4. Think about orientation
The part is built layer by layer. Orientation affects surface quality, the need for support structures and where layer lines fall. Tell us which surfaces are functional; we orient the part to protect them.
5. Let the slurry out
Closed cavities trap uncured slurry, which ruins the part during debinding. Hollow parts and channels need openings so slurry can drain and be cleaned out.
6. Holes, threads and inserts
Through holes print better than blind holes. Fine threads in ceramic are fragile; use a bonded or press-fit insert where a screw connection is needed.
7. Tolerances and datums
Define datum features on the drawing and mark critical dimensions. We measure them on our ZEISS PRISMO and include the results in the report.
Checklist before you send files
- A STEP file of the part, and a PDF drawing with tolerances and datums
- The material, or the conditions the part must survive
- Functional surfaces and critical dimensions marked
- Quantity now and expected volume later
- Any NDA you need us to sign first